Home / Products / Nickel Alloys / Inconel 625 / ASTM B366 Inconel 625 Threaded Fittings
                Inconel 625 (UNS: N06625, Werkstoff Nr.: 2.4856)
                Fabricated using stainless steel, our range of threaded fittings is one of the most demanded items of our entire range. Suitable for different industrial projects, these adroitly developed threaded pipe fittings are stringently checked for their durability and strength. These are also offered in accordance with the national and international standard & specifications.
                
                ASTM B366 Inconel 625 Threaded Fittings
                Specifications
                
                      
                        
                          | Standards | Designation | 
                        
                          | ASTM | B 366 | 
                        
                          | ASME | SB 366 | 
                      
                    
                
                    
                      
                        
                          | UNS | N06625 | 
                        
                          | Werkstoff Nr. | 2.4856 | 
                      
                    
                
                    
                Dimensions
                
                Chemical Composition
                
                      
                        
                          |  | Inconel 625 | 
                        
                          | Ni | 58.0 min | 
                        
                          | Cr | 20.0 – 23.0 | 
                        
                          | Fe | 5.0 max | 
                        
                          | C | 0.10 max | 
                        
                          | Mn | 0.50 max | 
                        
                          | Si | 0.50 max | 
                        
                          | Mo | 8.0 – 10.0 | 
                        
                          | Co | 1.0 max | 
                        
                          | Al | 0.40 max | 
                        
                          | Ti | 0.40 max | 
                        
                          | Nb + Ta | 3.15 – 4.15 | 
                        
                          | P | 0.015 max | 
                        
                          | S | 0.015 max | 
                      
                    
                Mechanical & Physical Properties – Inconel 625
                
                      
                        
                          | Density | 8.4 g/cm3 | 
                        
                          | Melting Point | 1350 °C (2460 °F) | 
                        
                          | Tensile Strength | Psi – 135,000 , MPa – 930 | 
                        
                          | Yield Strength (0.2%Offset) | Psi – 75,000 , MPa – 517 | 
                        
                          | Elongation | 42.5 % | 
                      
                    
                Subcategory: Metal; Nickel Base; Superalloy
                Key Words: ASME SB-443, SB-444, SB-446, SB-564, Boiler Code   Sections I, III, VIII, IX; AFNOR NC 22 D Nb; VdTUV 499, AMS 5581, AMS   5599, AMS 5666, AMS 5837; DIN 17744, 17750-17752, 17754; Werkstoff Nr.   2.4856; NACE MR-01-75, UNS N06625; BS 3072, 3074, 3076 (NA21); ASTM   B443, ASTM B444, ASTM B446, ASTM B564, ASTM B704, ASTM B705, ASTM B751
                
                      
                        | Component Al
 C
 Co
 Cr
 Fe
 | Wt. % Max 0.4
 Max 0.1
 Max 1
 20 - 23
 Max 5
 | 
                      
                        | Component Mn
 Mo
 Nb
 Ni
 | Wt. % Max 0.5
 8 - 10
 3.15 - 4.15
 Min 58
 | 
                    
                
                    
                      
                        
                          | Electrical Properties | 
                        
                          | Electrical Resistivity | 0.000129 ohm-cm | 0.000129 ohm-cm |  | 
                        
                          | Magnetic Permeability | 1.0006 | 1.0006 | at 200 oersted (15.9 kA/m) | 
                        
                          | Curie Temperature | Max -196 °C | Max -321 °F |  | 
                        
                          | Thermal Properties | 
                        
                          | CTE, linear 20°C | 12.8 µm/m-°C | 7.11 µin/in-°F | 20-100°C | 
                        
                          | Heat Capacity | 0.41 J/g-°C | 0.098 BTU/lb-°F |  | 
                        
                          | Thermal Conductivity | 9.8 W/m-K | 68 BTU-in/hr-ft²-°F |  | 
                        
                          | Melting Point | 1290 - 1350 °C | 2350 - 2460 °F |  | 
                        
                          | Solidus | 1290 °C | 2350 °F |  | 
                        
                          | Liquidus | 1350 °C | 2460 °F |  | 
                      
                    
                 
                
                Main Export Market
                
                      - Eastern Europe
- North America
- Mid East/Africa
- Central/South America
- Asia
- Western Europe
- Australasia
- UAE
Sales Locations 
                
                      U.A.E,
                        Oman,
                        Saudi Arabia,
                        Qatar,
                        Bahrain,
                        Egypt,
                        Turkey
                        Singapore,
                        Thailand,
                        Malaysia
                        Indonesia
                        Poland
                        Italy
                        Portugal
                        Spain
                        Brazil
                        Chile
                        Venezuela
                        Costa Rica
                        USA
                        Canada
                        Angola
                        Sri Lanka
                        Russia